I got a new weapon: DMT600 for beating blades in whimpering submission. So I figure I best hone something up, right?
Here is the progression of images (400x)
Here is the progression of images (400x)
- Factory edge
- DMT600 (new hone, not broken in whatsoever)
- DMT1200 (well used and loved, broken in like an old pair of jeans)
- 3um AlOx lapping film (used many, many times)
- 1um AlOx lapping film (also used on many a razor)
Attachments